Description 性能 |
Test Method 测试方法 |
判定标准 Typical value |
|
Shore A hardness 邵氏硬度A |
DIN ISO 7619-1(3S) |
85(+/-5) |
|
Tensile strength, 拉伸强度 |
TL 529-2008 1 6.2 & DIN 53504:2009 |
≥30N/mm2 |
|
Dimension change rate, 尺寸变化率 |
ES-2U5A-1A263-AA-2005 6.4 ,170℃,24h |
≤10% |
|
Abrasion, mm3 耐磨损 |
ES-2U5A-1A263-AA-2005 6.9 &ASTM D4060-2014 |
≤0.1% |
|
Flammability 燃烧测试 |
ES-2U5A-1A263-AA-2005 6.10 & ISO 3795:1989
|
≤100mm/min |
|
Low temperature resistance 耐低温 |
ES-2U5A-1A263-AA-2005 6.5 ,-40℃,4h |
No deformation and no break 无变形或开裂 |
|
High temperature 高温测试 |
GB/T2423.1-2008 |
No deformation and no break |
Temperature resistance 耐热性能 |
ES-2U5A-1A263-AA-2005 6.8 ,125℃,3000h |
No deformation and no break 无变形或开裂 |
Thermal aging test 热老化测试
|
ES-2U5A-1A263-AA-2005 6.3 ,125℃,400h |
≥35% |
|
Odor 气味 |
Refer FLTM BO 131-03 (2017) Sampling volume:3L,type:A ,Size:100cm²
|
WSS-M99P2222-F1 (2017) ≤3.0 |
|
VOC |
Refer FLTM BZ 108-01( 7/2/2018)VOC, (HPLC/DAD) (TDS/GC-MS) |
/ |
|
Nebulization 雾化 |
Refer SAE J1756(2006)
Reflection method :heating at 100 ℃ /3 hours . condensing temperature 21℃,Drying time 16 hours |
Based on WSS-M99P2222-F1(2017) Reflection method 反射法:≥70,无油膜、液滴、结晶状沉积物 |
|
Density 密度 |
TL 529-2008 1&DIN EN ISO 1183-1:2013 Method A
|
1.095g/cm3 |
|
ELV |
GB/T 30512-2014 |
铅(Pb)≤100ppm、镉(Cd)、汞(Hg)、六价铬(Cr6+)、多溴联苯(PBBs)、多溴二苯醚(PBDEs)≤1000ppm |
|
RoHS |
Refer RoHS Directive2011/65/EU and amending Annex directive EU 2015/863 |
铅(Pb)≤100ppm、 镉(Cd)、汞(Hg)、六价铬(Cr6+)、多溴联苯(PBBs)、多溴二苯醚(PBDEs)、DBP、BBP、DEHP、DIBP≤1000ppm |
|
Short term aging 短期老化 |
ISO 6722-1:2011
150 ℃,240 h→-25℃,4h |
No crack and no break |
|
Elongation at break 断裂伸长率 |
TL 529-2008 1 6.2 & DIN 53504:2009 |
≥400% |
|
IR 红外光谱 |
GB/T 6040-2019 |
≥95% |
|
Impact test抗冲击试验 |
ISO 6722-2011 |
No crack and no break |
|
Ozone resistance 耐臭氧试验 |
SMTC 3 261 004 |
'0 level , No crack |
|
Chemical resistance 耐化学试剂 |
SMTC 3 800 001-20109(V1) 10.2 |
No break |
|
Hydrolysis resistance 耐水解 |
500h storage in istilled water at 85℃ for 500h 85℃蒸馏水中存放
|
No crack and no break |
|
Crushed stone impact test碎石冲击试验 |
SAE J400-2012 |
No break and no scratch on the tube surface 套管表面无明显损坏、磨痕 |